简介:
简介:德国Ⅵ系统公司宣布研制出第一个通过多模光纤数据传输速率达40吉比特/s(40Gbit/s)的单VCSEL(垂直腔面发射激光器)。2009年1月份在美国加州SanJose召开的光子学会议上,该公司刚介绍了其20吉比特/s的器件,目前又使它的量子点激光器的调制速率提高了1倍。该公司利用其VCSEL和PIN光探测组件实现了通过多模光纤的40吉比特/s连续传输,这是850hm(波长)光发射的刨记录器件,是用与20吉比特/sVCSEL相同的光刻掩模研制的,但对外延结构作了改进。这种器件设计利用GaAs量子阱中的InAs量子点,并嵌入到AlGaAs基体中。
简介:Usingaspecialconstantdeflectiondevice,thechangesindislocationconfigurationaheadofaloadedcracktipfor60Fe40Nialloy,beforeandaftermagnetizationinamagneticfield,havebeenstudiedinTEM.Theresultsshowedthatthemagnetizationfor60Fe40Nialloycouldenhancedislocationemission,multiplicationandmotion.Also,themechanicalpropertiesof60Fe40Nialloy,inairandinthemagneticfieldrespectively,havebeeninvestigatedusingtheslowstrainratetension.Andtheresultsindicatedthatmagnetizationcouldmaketheyieldstrengthcorrespondingtodecreaseby26percent,butdidnotinfluencetheultimatetensilestrengthandthefracturestrain,whichshowedthatmagnetizationcouldenhanceplasticdeformation.
简介:以前曾指出由3,3’,4,4’-联苯基四羧酸二酐(BPDA)和1,2-双(4-氨基苯氧基)苯(亦称三苯基醚邻苯二酚二胺(TPEC))衍生的聚酰亚胺具有优异的拉伸性能和良好的热性能。本文对由BPDA、TPEC及其它芳香族二胺制备的共聚酰亚胺的性能做了初步评价。由BPDA和各种芳香族二胺制备的均聚酰亚胺通常具有良好的机械性能和热性能。然而,它们不溶于现有的各种有机溶剂中。在某些条件下,用BPDA与等摩尔TPEC和其它芳香族二胺混合物可以制备可有机溶解的BPDA型共聚酰亚胺。这些共聚酰亚胺可以形成坚韧的薄膜,它们具有较高的模量和强度。多数情况下,也具有较高的断裂伸长率。
简介:TheW-Cucompositesarewidelyusedasweld-ingelectrodes,electronicpackagingmaterials,electricdischargematerialsandheatsinksbecauseoftheexcellentproperties.Inthisresearch,theW-40wt.%Cucompositeswerepreparedthroughthevacuumhot-presssinteringmethod,andtheeffectofsinteringtemperatureonthemicrostructureand
简介:TheeffectoftitaniumadditiononthemicrostructureandmechanicalpropertiesofbrassCu40Znhasbeenstudiedviathepowdermetallurgy(P/M)route.Thewater-atomizedCu40Zn—1.0wt%Tialloypowderwasconsolidatedatdifferenttemperaturesintherangeof400—600℃usingsparkplasmasintering(SPS)andhotextrusionsubsequently.Resultsshowthatthesuper-saturatedsolidsolutiontitaniumelementinrapidlycooledbrassCu40Znpowdercreatedhighchemicalpotentialforaprecipitatereaction,showingsignificantgrainrefinementeffectsontheconsolidatedCu40Znmatrix.Consequently,excellentmechanicalpropertieswereobtainedbyprecipitationhardeningandworkhardeningaftersinteringandextrusion,withyieldstrengthof390MPa,ultimatetensilestrengthof617MPa,andVickersmicro-hardnessof192HV,whichare28.7%,23.4%,and23.9%highervaluesthanthoseofextrudedCu40Znbrass,respectively.