简介:采用金相组织观察、力学性能测试和统计分析等手段,研究了成品退火工艺对Φ5mmTP2内螺纹铜管微观组织和力学性能影响规律。结果表明:Φ5mmTP2内螺纹铜管退火温度为470~480℃时,铜管组织细小、均匀,同时能获得较高塑性和较高强度;490~500℃时,铜管晶粒尺寸、力学性能波动大;510~520℃时,铜管组织易粗大。Φ5mmTP2内螺纹铜管在470℃退火时,晶粒尺寸随退火时间的规律变化为d=0.0008t3-0.062t^2+1.7t-1.3,保温21min时,铜管再结晶基本完成,保温时间为28~31min时,铜管组织状态和综合力学性能最佳。
简介:Improvingtheunitheatefficiency,reducingcoalconsumptionandtheemissionofCO2andmeetingtherequirementsofenvironmentalprotectionandenergyconservationisthegoaloftheboilerandthepowerindustry.Developmentsoflargecapacityandhighparameterultra-supercritical(USC)unitsarethetendencyofthepowerindustry.ThereisnodoubtthatthedevelopmentofUSCunitsisbasedonthedevelopmentofmaterials,especiallythematerialsusedforsuper-heaterandreheaterinhigh-temperatureUSCboiler.Duetothelongtimeexposuretotheharshenvironment,suchasbearingthe600℃steamoxidation,andwithstandingthecorrosivefluegasandflyasherosion,thematerialsrequirenotonlygoodhigh-temperaturestrength,butalsoagoodcorrosionresistance.Inconsiderationoftherequirementscitedabove,foreigncountrieshaddevelopedTP310HCbN(07Cr25Ni21CbN)austeniticheat-resistantsteel.However,thedomesticdemandsforthismaterialstilldependonimportandthecostishigh,sotheboilerandthepowerindustryexpectseagerlythatthesesteelscanbeproducedbydomesticmetallurgicalindustry,especiallyBaosteel,toreplacetheimportedproducts.Inordertosatisfytherequirementsofdomesticmanufacturingsuper-heaterandreheaterusedinultra-supercriticalpowerboiler,afterdevelopedT23、T91、T92、S30432highpressureboilertube,BaosteelbegantodevelopTP310HCbN(07Cr25Ni21CbN)austeniticstainlesssteeltubeinJanuaryof2007.Thisstudydescribesthecompositiondesign,themanufacturingprocessofproduct,andtheassessmentofperformanceofBaosteel’sTP310HCbN(07Cr25Ni21CbN).ThedataindicatesthatpropertiesofBaosteel’sTP310HCbN(07Cr25Ni21CbN)conformtotheASMESA-213standardandGB5310standard,soitcansubstitutetheimportedproductsandissuitableformanufacturingpowerstationboilerofgreatcapacityandhighsteamparameters.